Type: | Diamond |
---|---|
Classification of Diamond: | Artificial |
Characteristic: | High Thermal Stability |
Characteristics of Natural Diamond: | Compressive Strength |
Application: | Machinery and Electronics |
Product Name: | CVD Single Crystal Diamond Plate |
Samples: |
---|
Customization: |
---|
Suppliers with verified business licenses
The advantages of CVD diamond growth include the ability to grow diamond over large areas and on various substrates, and the fine control over the chemical impurities and thus properties of the diamond produced. Unlike HPHT, CVD process does not require high pressures, as the growth typically occurs at pressures under 27 kPa
Size of CVD diamond plates:
Normal size of CVD diamond plates:
3*3*1mm | 4*4*1mm | 5*5*1mm | 6*6*1mm | 7*7*1mm | 8*8*1mm |
3*3*0.5*mm | 4*4*0.5mm | 5*5*0.5mm | 6*6*0.5m | 7*7*0.5mm | 8*8*0.5mm |
4*2*1mm | 5*3*1mm | 5*4*1mm | 6*3*1mm | 6*4*1mm | 6*3*1mm |
Thickness of diamond plates:from 0.3mm to 3mm
Advantages
Crystal growth process: | CVD diamond optical laser cuting cylinder |
Color: | Optical grade- Colorless, |
Mechanic grade - Brownish | |
Advantage: | 1) Regular shape, uniform size. The size can be strictly controlled according to customer needs. 2) High repurchase rate and high cost performance, well received by customers. |
Orientation: | 4pt/100 |
2pt/110 | |
Shape: | Square |
Lateral Dimensions Measured | to smaller side |
Edges | Laser Cut |
Laser Kerf | < 3° |
Lateral Tolerance: | +0.1/-0 mm |
Roughness, Ra | Two sides polished, Ra < 30 nm |
Thickness Tolerance | +/- 0.05 mm |
Boron Concentration [B]: | <0.05 ppm |
Nitrogen Concentration: | Optical grade <10ppm |
Mechanical grade - <50 ppm |